Efecto de la relación área-volumen en la sinterización de varistores cerámicos basados en ZnO-Bi2O3

Show simple item record

dc.contributor Comisión Interministerial de Ciencia y Tecnología, CICYT (España)
dc.creator Rubia, Miguel Ángel de la
dc.creator Peiteado, Marco
dc.creator Fernández Lozano, José Francisco
dc.creator Caballero Cuesta, Amador
dc.date 2008-06-02T10:55:16Z
dc.date 2008-06-02T10:55:16Z
dc.date 2002-01
dc.date.accessioned 2017-01-31T01:32:02Z
dc.date.available 2017-01-31T01:32:02Z
dc.identifier Boletín de la Sociedad Española de Cerámica y Vidrio 41(1) 194-197 (2002)
dc.identifier 0366-3175
dc.identifier http://hdl.handle.net/10261/4715
dc.identifier.uri http://dspace.mediu.edu.my:8181/xmlui/handle/10261/4715
dc.description [ES] La sinterización de varistores cerámicos basados en el sistema ZnO-Bi2O3-Sb2O3 requiere temperaturas del orden de 1150- 1200ºC y ocurre en presencia de una fase líquida rica en Bi2O3 que se forma entre 700 y 800ºC dependiendo de la composición concreta del material. La volatilización incontrolada de Bi2O3 puede alterar notablemente la respuesta eléctrica del material, ya que este componente resulta crítico para la configuración de los bordes de grano activos. Por otro lado, la completa oxigenación del material durante la sinterización también resulta determinante en la respuesta eléctrica final del varistor. Consecuentemente, la relación área-volumen de los compactos en verde se convierte en un parámetro relevante durante la sinterización del material. En el presente trabajo se han estudiado las características microestructurales y la respuesta intensidad- voltaje de varistores cerámicos de idéntica composición, sinterizados a partir de compactos con diferente relación áreavolumen. Se ha observado que, dependiendo de la temperatura de sinterización, existe un valor de la relación área-volumen a partir del cual la respuesta eléctrica del material se degrada dramáticamente.
dc.description [EN] Sintering of ceramic varistors based on the system ZnO-Bi2O3-Sb2O3 takes place at 1150-1200ºC in the presence of a Bi-rich liquid phase which forms at 700-800ºC, depending on the exact material composition. Uncontrolled bismuth oxide volatilisation can modify the electrical response of the material since bismuth is critical for the development of the electrically active grain boundaries. On the other hand, material oxygenation is also essential for the electrical behaviour of the material. Consequently the area-volume ratio of the green compacts becomes a relevant parameter for the sintering process. In the present work, the microstructure and current-voltage characteristic of sintered varistors with different area-volume ratio and identical composition have been studied. Depending on the sintering temperature, there is value for the area-volume ratio above which a strong decrease of the electric properties of the varistor device is observed.
dc.description Este trabajo ha sido realizado en el marco del proyecto C00 1999 AX012 (CICYT). Los autores agradecen a INAEL S.A., KERABEN S.A., IKV S.A., IQB S.A., y al CSIC el apoyo prestado en la realización del trabajo.
dc.description Peer reviewed
dc.format 412857 bytes
dc.format application/pdf
dc.language spa
dc.publisher Sociedad Española de Cerámica y Vidrio
dc.relation http://boletines.secv.es/es/index.php?id=42&vol=41
dc.rights openAccess
dc.subject Varistor cerámico
dc.subject Relación área-volumen
dc.subject Sinterización
dc.subject Respuesta eléctrica
dc.subject Ceramic varistor
dc.subject Area-volume ratio
dc.subject Sintering
dc.subject Electrical properties
dc.title Efecto de la relación área-volumen en la sinterización de varistores cerámicos basados en ZnO-Bi2O3
dc.title Effect of the area-volume ratio in the sintering of ZnO-Bi2O3 based ceramic varistors
dc.type Artículo


Files in this item

Files Size Format View

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record

Search DSpace


Advanced Search

Browse

My Account